Steel / M35
M35
M2 with five percent cobalt, for heat that would soften a plain edge.
Taps, drills and end mills for stainless and heat-resistant steels at higher speeds.
ISOHS6-5-2-5
Co %4.50 to 5.00
FormsIngot, charge mix, Powmex bar
Reference chemistry
Percent by weight, as EN ISO 4957 sets them for M35. Our ingot is sold as remelt feed, and each heat's own analysis goes with it.
Hot hardness
Toughness
Wear resistance
| Element | Min | Max |
|---|---|---|
| C | 0.87 | 0.95 |
| Mn | 0.40 | |
| Si | 0.45 | |
| Cr | 3.80 | 4.50 |
| V | 1.70 | 2.10 |
| W | 5.90 | 6.70 |
| Mo | 4.70 | 5.20 |
| Co | 4.50 | 5.00 |
| P | 0.030 | |
| S | 0.030 |
Equivalent names
EN ISO 4957HS6-5-2-5
Werkstoff1.3243
JIS G4403SKH55
GB/T 9943W6Mo5Cr4V2Co5
ASTM A600Not an A600 type